TECHNET Archives

October 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Bob Wettermann <[log in to unmask]>
Date:
Tue, 22 Oct 2013 10:21:01 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bob Landman <[log in to unmask]>
Message-ID:
Subject:
From:
Bob Landman <[log in to unmask]>
MIME-Version:
1.0 (1.0)
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (31 lines)
Bob,

McMaster Carr supplies a Teflon epoxy system which has a liquid etchant to prepare the surface for their two component epoxy. Its packaged in a circular cardboard box with a screw top lid.  We've used it to bond Teflon to aluminum for decades. Don't know if it works on epoxy/resin boards but as it can bind Teflon to Teflon (another app we have a requirement for) give them a call to see what they recommend.

Bob Landman
H&L Instruments,LLC


Sent from my iPhone

On Oct 22, 2013, at 10:09 AM, Bob Wettermann <[log in to unmask]> wrote:

> Can a chemist/board SME tell me if an epoxy/resin system will bond to a PTFE
> matrix laminate for pad/trace repair?
> 
> Thanks!
> 
> Bob Wettermann
> 
> 
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask] 
> ______________________________________________________________________
> 

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2