TECHNET Archives

March 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Fri, 13 Mar 1998 21:38:50 EST
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Hint pwb1 <[log in to unmask]>
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
Hint pwb1 <[log in to unmask]>
Content-transfer-encoding:
7bit
Parts/Attachments:
text/plain (30 lines)
Sheila,

Looking at the recently issued copy of IPC-4101 on page 19 it give a cross
reference between Nema, MIL-S-13949 and the specification sheets in IPC-4101.
GIN is #40, GIL is #41 and GIJ is # 42.  The IPC-4101 puts the laminate and
prepreg under a single # while the MIl Spec put the GI prepreg under a /13
instead of GIL, GIN or GIJ.  However, if you use the mil spec you should
designate the characteristics as PGIL, PGIJ or PGIN by using the designators
called out in Par. 1.2.1.2 and specify per the slash sheet 13. which is for GI
(generic) only.  If you specified MIL-S-13949/13, you would also add the J or
L designators as required by the /13 slash sheet.

With the IPC-4101 you specify the prepreg to be Spec # __ with the
reinforcement, resin flow, gel time, resin content, etc. stated on your
procurement documentation.

Phil Hinton

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2