TECHNET Archives

February 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Les Connally <[log in to unmask]>
Reply To:
Les Connally <[log in to unmask]>
Date:
Fri, 26 Feb 1999 15:15:46 -0600
Content-Type:
Multipart/Mixed
Parts/Attachments:
text/plain (1653 bytes) , ATTRIBS.BND (3991 bytes)
Hi Bryan,

I'm Curious as to what Class copper you are using on the Inner layers. We have
found that in the past that class-1 copper would not cut it, and switched to
Class-3 Copper which is more ductile. This practically eliminated foil
cracking.

Regards,
Les
>  From: Bryan Kerr +44 1383 822131 ext 4409 <[log in to unmask]>, on 2/25/99
>  4:58 PM:
>  On this subject, I have recently been investigating an open circuit problem
>  with a multilayer board and have found a small, but significant, level of
>  foil
>  cracking at the hole / inner layer interface with no apparent reason. There
>  are
>  no unused pads and I had already been pondering whether the lack of these
>  "dummy" pads could result in more stress on the inner layer junctions during
>  thermal shock - 288 C for 10 seconds. Maybe any weaknesses in the junction
>  are
>  more likely to result in fracture if there are no dummy pads ?
>  Comments, anybody.
>
>  Bryan
>
>  ################################################################
>  TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>  ################################################################
>  To subscribe/unsubscribe, send a message to [log in to unmask] with following
>  text in the body:
>  To subscribe:   SUBSCRIBE TechNet <your full name>
>  To unsubscribe:   SIGNOFF TechNet
>  ################################################################
>  Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
>  for additional information.
>  For technical support contact Hugo Scaramuzza at [log in to unmask] or
>  847-509-9700 ext.312
>  ################################################################
>
>


ATOM RSS1 RSS2