TECHNET Archives

July 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Baski Devre <[log in to unmask]>
Date:
Thu, 13 Jul 2006 17:14:47 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, R Sedlak <[log in to unmask]>
Subject:
From:
R Sedlak <[log in to unmask]>
Content-Transfer-Encoding:
8bit
In-Reply-To:
Content-Type:
text/plain; charset=iso-8859-1
MIME-Version:
1.0
Parts/Attachments:
text/plain (246 lines)
I do not know the names of the oils sold by various chemical vendors.
May I suggest trying to contact them, and not asking for an oil for roller tinning, as this is not a common process, but ask for an oil for fusing, or reflow, which used to be a very common practice.

Alternately, you can purchase Ammonium Chloride, and Zinc Chloride, and simply mix them together.  This would work quite well, after you had experimented to find out how much of each to use.

Do you have a MacDermid rep you are in contact with?   I can find out the name of their oil.

Rudy Sedlak
RD Chemical Company

Baski Devre <[log in to unmask]> wrote: Dear Sedlak
Sorry please do not misunderstand I think salt sources of alfa is about
to exhaust or they gave up producing this salt. But I have not heard of
water soulable oil used in roller tinning proces to reduce dross
formation. Can you give me contact mail or water soulable oil
Thanks again and again
Yusuf
R Sedlak yazmış:

>Yusuf Gomec:
>  The type of oil you want is effectively the same sort which we used to use to fuse, or reflow, boards, a long long time ago, and I suspect there are many people who can supply it, but the closest to you is probably Alfachimici, in Italy.
>
>  Rudy Sedlak
>  RD Chemical Company
>
>Baski Devre  wrote:
>  Dear Sedlak and Mike
>Is it possible for you to give us more info about water soluble oil and
>do you have any brand that you will suggest us
>Best Regards
>
>Yusuf GÖMEÇ
>Product Quality Engineer
>
>
>BASKI DEVRE SAN ve TIC LTD STI
>Ceyhan Sk. No:10 34896 Pendik-Istanbul-Turkey
>Tel: 00 90 216 3901036 (4 Hat/Line)-173(Extention)
>00 90 216 4836560 (4 Hat/Line)-173(Extention)
>Fax: 00 90 216 3544941
>00 90 216 4913269
>Gsm: 00 90 533 6579897
>00 90 533 7480014
>msn: [log in to unmask]
>
>
>
>R Sedlak yazmış:
>
>
>
>>Thanks for the explanation... I have heard/seen water soluble oil being used in roller tinning, and it apparently worked well.. have never heard of salt being used until now.
>>
>>Rudy Sedlak
>>
>>Mike Fenner wrote:
>>The salt controls dross on the pot and (sometimes forgotten) ensures the
>>bottom roller remains tinned. The alternative to salt is vigilance and more
>>dross. Possibly you could use a [so called] water soluble oil, but I have
>>never seen this done, as these were introduced after roller tinning fell out
>>of use in Europe.
>>Roller tinning is an old process, but cheap. I think the nearest modern
>>equivalent process, to think of as an alternative, would be Hot Air Solder
>>Levelling. This would give much better or at least consistent solderability
>>and not have the blips on the trailing edge of pads.
>>
>>
>>Regards
>>
>>Mike Fenner
>>Indium Corporation
>>
>>T: + 44 1908 580 400
>>M: + 44 7810 526 317
>>F: + 44 1908 580 411
>>E: [log in to unmask]
>>W: www.indium.com
>>Pb-free: www.Pb-Free.com
>>
>>
>>
>>
>>-----Original Message-----
>>From: TechNet [mailto:[log in to unmask]] On Behalf Of Baski Devre
>>Sent: 12 July 2006 16:39
>>To: [log in to unmask]
>>Subject: [TN] Roller Tinning Process
>>
>>Dear Technetters
>>As you know that some PCB manufacturer uses roller tinning soldering
>>process. In this process firstly flux is spread over PCB and then passed
>>through rollers to be soldered. In this solder alloy sometimes a bit
>>salt is added to improve soldering quality and help solder to be appread
>>bright. I want to learn that if there is any alternative material used
>>in roller tinning soldering process to elaminate salt or is there any
>>alternative roller tinning soldering process flow.
>>Thanks in advance to your comments and knowledge share
>>Best Regards
>>
>>--
>>Yusuf GÖMEÇ
>>Product Quality Engineer
>>
>>
>>BASKI DEVRE SAN ve TIC LTD STI
>>Ceyhan Sk. No:10 34896 Pendik-Istanbul-Turkey
>>Tel: 00 90 216 3901036 (4 Hat/Line)-173(Extention)
>>00 90 216 4836560 (4 Hat/Line)-173(Extention)
>>Fax: 00 90 216 3544941
>>00 90 216 4913269
>>Gsm: 00 90 533 6579897
>>00 90 533 7480014
>>msn: [log in to unmask]
>>
>>---------------------------------------------------
>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>>To unsubscribe, send a message to [log in to unmask] with following text in
>>the BODY (NOT the subject field): SIGNOFF Technet
>>To temporarily halt or (re-start) delivery of Technet send e-mail to
>>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>>To receive ONE mailing per day of all the posts: send e-mail to
>>[log in to unmask]: SET Technet Digest
>>Search the archives of previous posts at: http://listserv.ipc.org/archives
>>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>>for additional information, or contact Keach Sasamori at [log in to unmask] or
>>847-615-7100 ext.2815
>>-----------------------------------------------------
>>
>>
>>***This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.
>>
>>Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***
>>
>>---------------------------------------------------
>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>>To unsubscribe, send a message to [log in to unmask] with following text in
>>the BODY (NOT the subject field): SIGNOFF Technet
>>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>>Search the archives of previous posts at: http://listserv.ipc.org/archives
>>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>>-----------------------------------------------------
>>
>>
>>
>>---------------------------------
>>
>>---------------------------------------------------
>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>>To unsubscribe, send a message to [log in to unmask] with following text in
>>the BODY (NOT the subject field): SIGNOFF Technet
>>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>>Search the archives of previous posts at: http://listserv.ipc.org/archives
>>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>>-----------------------------------------------------
>>Talk is cheap. Use Yahoo! Messenger to make PC-to-Phone calls. Great rates starting at 1¢/min.
>>
>>
>>
>>
>
>
>--
>Yusuf GÖMEÇ
>Product Quality Engineer
>
>
>BASKI DEVRE SAN ve TIC LTD STI
>Ceyhan Sk. No:10 34896 Pendik-Istanbul-Turkey
>Tel: 00 90 216 3901036 (4 Hat/Line)-173(Extention)
>00 90 216 4836560 (4 Hat/Line)-173(Extention)
>Fax: 00 90 216 3544941
>00 90 216 4913269
>Gsm: 00 90 533 6579897
>00 90 533 7480014
>msn: [log in to unmask]
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>-----------------------------------------------------
>
>
>
>---------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>-----------------------------------------------------
>Yahoo! Music Unlimited - Access over 1 million songs.Try it free.
>
>


--
Yusuf GÖMEÇ
Product Quality Engineer


BASKI DEVRE SAN ve TIC LTD STI
Ceyhan Sk. No:10 34896 Pendik-Istanbul-Turkey
Tel: 00 90 216 3901036 (4 Hat/Line)-173(Extention)
     00 90 216 4836560 (4 Hat/Line)-173(Extention)
Fax: 00 90 216 3544941
     00 90 216 4913269
Gsm: 00 90 533 6579897
     00 90 533 7480014
msn: [log in to unmask]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------



---------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Yahoo! Messenger with Voice. Make PC-to-Phone Calls to the US (and 30+ countries) for 2¢/min or less.

ATOM RSS1 RSS2