TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Honsowetz, Eric" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Honsowetz, Eric
Date:
Mon, 18 Sep 2006 14:59:06 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (122 lines)
Well that depends...

For discrete components such as resistors etc that is a correct
statement, however many of the IC's have needed to change packaging
material to meet the higher temperatures of SAC.

eric

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Monday, September 18, 2006 2:28 PM
To: [log in to unmask]
Subject: Re: [TN] Lower temp soldering pass of lead-free boards

Hi Ioan!

Are you sure that things are really different between the "Leaded" and
"Lead-free" parts besides the plating? We were in a situation where we
had to build a consigned material assembly which is in the process of
becoming "compliant". However, our customer had purchased quite a number
of digital video devices and did not want to throw them away because
they weren't PB free...the assemblies that we were building weren't
going to the EU.

But we were using PB free solder paste and had some concerns about
whether or not the leaded parts would be able to withstand the lead-free
temperatures. So we called the manufacturer of the device inquiring if
the part could take the heat, and was told "unofficially" (like if we
repeated what he said he would deny it) that the only difference between
the lead-free and leaded part was the plating on the leads...nothing had
changed internally.

I wonder how many PB free parts REALLY have something different about
them besides the lead plating?

-Steve Gregory-

 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan
Sent: Monday, September 18, 2006 11:26 AM
To: [log in to unmask]
Subject: [TN] Lower temp soldering pass of lead-free boards

Hi Technos,

I have a lead-free board, but some nasty leadless comps are only
available leaded, so not supporting 240C.

I am thinking what about soldering everything that works at lead-free
temps and then make another soldering pass at about 210C with these
comps only. Will this affect the reliability of the lead-free joints,
since the solder will get almost pasty? Did anybody try this?

I agree with the ones that will say: "what the heck, they cannot give
you compliant parts, don't do it", but it is an important project, the
customer knows what this means, but they want to risk.

Btw, I have to make sure the original reliability of the lead-free
joints, as good as it is, will not be latered, it is a high-rel
application.

Thanks,

Ioan

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

**********************
** LEGAL DISCLAIMER **
**********************

This E-mail message and any attachments may contain

legally privileged, confidential or proprietary

information. If you are not the intended recipient(s),
or the employee or agent responsible for delivery of

this message to the intended recipient(s), you are

hereby notified that any dissemination, distribution

or copying of this E-mail message is strictly

prohibited. If you have received this message in

error, please immediately notify the sender and

delete this E-mail message from your computer.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2