What concentration of HCl is used?

Ryan

>-----Original Message-----
>From:  Larry Tawyea [SMTP:[log in to unmask]]
>Sent:  Tuesday, December 21, 1999 11:52 AM
>To:    [log in to unmask]
>Subject:       Re: [TN] HCl clean of Ni/Au plating
>
>In a message dated 12/21/99 11:20:32 AM Central Standard Time,
>[log in to unmask] writes:
>
><< Hello Technetters,
>
>         Is HCl clean of the nickel pads sometimes a step in the Ni/Au
> plating process? If it is, why is it done?
>  >>
>
>Craig,
>
>When you say plating the nickel pads I'm going to assume you are doing a
>selective plate as opposed to a pattern plate,  In this case there are
>process steps between the nickel and gold plate.  The purpose of the HCl
>clean is to remove the nickel oxide that forms very quickly when the nickel
>is exposed to air.  Hope this answers your question.
>
>Larry Tawyea
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in
>the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2