TECHNET Archives

November 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Peter L <[log in to unmask]>
Date:
Wed, 21 Nov 2007 07:27:58 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (62 lines)
Hello, Peter
I have a client using Loctite 3621 epoxy in a very similar application.
It bonds to the mylar sleeving very well. Try it.  

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Peter L
Sent: Tuesday, November 20, 2007 6:00 PM
To: [log in to unmask]
Subject: [TN] Epoxy application

Hello,
 
I would like to ask for opinion on an epoxy application. We apply RTV to
bond and secure 2 electronic devices on a PCB. 

But after noticing the RTV bond breaking off during vibration test, our
customer has specs in a 5min 2-part epoxy (made by
http://www.devcon.com/techinfo/5_MINUTE_FR.pdf) to replace the RTV. The
problem is that the Devcon epoxy is fast cure, requries 2 part mixing,
and carries a strong, irritating odor. I would like to move away from
using Devcon and expect that there must be more process friendly epoxy
for such application.

The 2 materials to be joined were a flat ferrite inductor and round
capacitor having a PVC sleeve. Due to positioning of the 2 devices there
is generally a ~0.25" gap between them for the epoxy to fill. The epoxy
bead deposit is about .75" long x 0.5" wide. (see following link to the
assembly
http://members.shaw.ca/ppwlee4/Epoxy_appl.JPG)

I am looking for recommendation of a suitable epoxy to allow:
 
- 5-10 min working life before it starts curing
- process friendly (smell, preferrable no pre-mix)
- good adhesion to the component/PCB surfaces.

Any suggestion is appreciated. Thanks.


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2