Paul, the committee updated the terminals soldering section to align to
IPC-A-610D and J-STD-001D terminal soldering criteria, including support
for lead free connections.
A new chapter was added that addresses electrical and mechanical
testing.
The molding/potting chapter was significantly expanded, lots of new
pictures and criteria.
The splicing section was significantly expanded with criteria for
heat-shrinkable solder splices added.
Numerous tweaks on verbage for clarification/ease of understanding. The
revision was nearly five years in development (originally published Jan
2002) and industry provided good comments for this revision.
Jack Crawford
IPC director certification and assembly technology
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stolar, Paul W
Sent: Tuesday, August 01, 2006 3:39 PM
To: [log in to unmask]
Subject: [TN] IPC-620
I just found out that the IPC/WHMA-A-620 was just revised.
Does anyone know what they changed?
Paul Stolar
Materials/Reliability Engineer
Manufacturing Reliability Lead Engineer
Baker Atlas
713-625-5376
713-625-4949 (fax)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|