TECHNET Archives

April 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wGpxJ-000BilC; Mon, 14 Apr 97 12:54 CDT
Content-Type:
text/plain; charset="us-ascii"
Old-Return-Path:
Date:
Mon, 14 Apr 1997 14:06:21 -0400
Precedence:
list
Resent-From:
Message-ID:
MIME-Version:
1.0
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/11934
From [log in to unmask] Mon Apr 14 16:
04:08 1997
TO:
Return-Path:
<TechNet-request>
X-Status:
Resent-Message-ID:
<"L6swW.0.EIB.8zcKp"@ipc>
Subject:
From:
"Baker,Kelly" <[log in to unmask]>
X-Loop:
Content-Transfer-Encoding:
7bit
X-Mailer:
Microsoft Exchange Server Internet Mail Connector Version 4.0.837.3
Resent-Sender:
TechNet-request [log in to unmask]
Parts/Attachments:
text/plain (107 lines)
Hey Denis, how goes the battle?  After long research, into immersion 
gold, the answer
to your question is no.  We use an auto catalytic, therefore, it an 
electroless system.  
If there's anyone else out there looking for indepth answers to 
immersion gold, save your time.  After hours of research basically it 
comes down to this, there's no spec to test it and there's
no spec to ref it.  There are 55110D, 6012, 45204, but they are of no 
real help.  I spoke with
Lisa Williams and Dave Corbett, who were very helpful, but the specs 
were not in the
depth that we were hoping for.  Thanks so much for trying to help.

----------
From:  Denis Meloche[SMTP:[log in to unmask]]
Sent:  Monday, April 14, 1997 10:02 AM
To:  Baker,Kelly
Subject:  Re: specifications (fwd)

Me again.  I think immersion gold is a general term for any plating 
process
where gold is suspended in liquid solution and plated through electro 
or
electroless process.  

At 12:11 PM 4/10/97 -0500, you wrote:
>
>
>---------- Forwarded message ----------
>Date: Wed, 9 Apr 1997 14:33:24 -0400
>From: Baker,Kelly <[log in to unmask]>
>To: "[log in to unmask]" <[log in to unmask]>
>Subject: specifications
>
> 
>Hi!
>
>Does anyone know of any Military of non Military specs for immersion 
>gold?  We know of the IPC-6012.  Any information would be appreciated.
>
>
>Thanks,
>
>Kelly
>
>**********************************************************************  
*****
>* TechNet mail list is provided as a service by IPC using SmartList 
v3.05 *
>**********************************************************************  
*****
>* To subscribe/unsubscribe send a message <to: 
[log in to unmask]>   *
>* with <subject: subscribe/unsubscribe> and no text in the body. 
         *
>**********************************************************************  
*****
>* If you are having a problem with the IPC TechNet forum please 
contact   *
>* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] 
     *
>**********************************************************************  
*****
>
>
>**********************************************************************  
*****
>* TechNet mail list is provided as a service by IPC using SmartList 
v3.05 *
>**********************************************************************  
*****
>* To subscribe/unsubscribe send a message <to: 
[log in to unmask]>   *
>* with <subject: subscribe/unsubscribe> and no text in the body. 
         *
>**********************************************************************  
*****
>* If you are having a problem with the IPC TechNet forum please 
contact   *
>* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] 
     *
>**********************************************************************  
*****
>
>
>
Denis Meloche
Technical Sales Engineer
Heraeus Cermalloy Division
24 Union Hill Rd
West Conshohocken Pa., 19428
610-825-6050 Fax 610-825-7061
E-Mail [log in to unmask]


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2