TECHNET Archives

August 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Bev Christian <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 17 Aug 2012 13:48:16 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Message-ID:
Subject:
From:
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-7"
Parts/Attachments:
text/plain (95 lines)
Bev,
Knowing me what do you think? The nobility of the mind as well as the metal can not always be easily washed away (disillusionment/dissolution).
Dewey

-----Original Message-----
From: Bev Christian [mailto:[log in to unmask]] 
Sent: Wednesday, August 15, 2012 5:54 PM
To: 'TechNet E-Mail Forum'; Whittaker, Dewey (EHCOE)
Subject: RE: [TN] gold removal question - to remove or not?

:) Dewey,
Was that intentional?  Wrong use of the word "disillusionment".

Graham,
I agree with Dewey that it is certainly overkill for PTH parts.  For SMT
parts, have you done the math to figure out % Au in a completed SMT joint
with different thicknesses of gold?  

Bev
RIM

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey (EHCOE)
Sent: Wednesday, August 15, 2012 3:44 PM
To: [log in to unmask]
Subject: Re: [TN] gold removal question - to remove or not?

Graham,
OK, we'll consider you a dip until proven otherwise. I hope you are talking
about SMT components? There is a good case for not pre-tinning (sounds more
technical than dip) PTH parts where there is a reasonable expectation of
disillusionment of the gold in your flow solder process.
Dewey 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Collins
Sent: Wednesday, August 15, 2012 12:16 PM
To: [log in to unmask]
Subject: [TN] gold removal question - to remove or not?

Hello Technet

I'm in the midst of a debate about gold removal.  Our policy on component
leads is to double dip tin all gold.  J-STD-001 says I do not have to do it
if there is less than "2.54 ìm [100 ìin]" of gold, but is it realistic to
operate on that basis?  For example, looking at an Airborne brand connector
I find the spec sheet says that there will be 50 ìin gold, minimum. Which is
not totally helpful as it does not tell me maximum.  I'm assuming given the
price of gold that they aren't looking to put a lot more than the minimum
on, but how controllable is the process?  Could we check the thickness once
and assume we are safe?

 

(and as you can tell from my phrasing I'm of the more conservative camp on
this one, still dipping the parts until proven wrong)

 

regards, 
  
Graham Collins 
Halifax Production Engineering 
(902) 873-2000 ext. 6215 

 

This message and any attachments are solely for the use of the individual or
entity to which it is addressed and may contain information that is
privileged or confidential or controlled technical data that is subject to
the laws of Canada or the United States. If you are not the intended
recipient, any disclosure, use or distribution of the information contained
herein is prohibited. If you have received this communication in error,
please notify the sender by reply e-mail and immediately delete this message
and any attachments.

 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2