By far the best protection of any kind of coating
Very uniform thickness, even over sharp edges and points
The vacuum/plasma reduces residual surface contamination, especially
hygroscopic volatiles
A bugger for rework
Expensive
GREAT!
Brian
Reuven ROKAH wrote:
> Hi Perylene users,
>
> Can you share with your experience and inform the + and - of this process?
>
> I have last week visited one of the users site and it seems promising.
>
> I have long experience with spraying systems and not vacuum systems.
>
> Best Regards
>
> Reuven
>
>
>
>
> Graham Naisbitt
> <Graham.Naisbitt@CON To: [log in to unmask]
> COAT.CO.UK> cc:
> Sent by: TechNet Subject: Re: [TN] Foreign material on top of the conformal coating
> <[log in to unmask]>
>
>
> 12/12/2003 18:02
> Please respond to
> "TechNet E-Mail
> Forum."; Please
> respond to Graham
> Naisbitt
>
>
>
>
>
> Bruce
>
> If you are applying epoxies and other materials after conformal coating,
> just be sure that the solvents (if any) are not affecting the coating
> during
> their application and curing.
>
> Otherwise this should simply be regarded as a cosmetic issue.
>
> Cleaning after all these processes is unlikely to be a good option, as the
> coating will now be expected to withstand your cleaning process...and
> surface cleaning using brushes, swabs etc., are only likely to be moving
> the
> stuff around on the surface rather than removing it.
>
> Hope this helps
> --
> Regards Graham Naisbitt
>
> [log in to unmask]
>
> Cell: 079 6858 2121
> Office: +44 (0)1252 813706
>
> Concoat Limited - Engineering Reliability in Electronics
>
> NEW - HumiSeal 1H2O Bov Aerosol - NEW
>
> Web: www.concoat.co.uk and www.concoatsystems.com
>
>
>
>>Hey guys,
>> I have be hit recently on a couple of occasions by the quality folks
>>over "foreign material" that is present on CCA's after conformal coating.
>>On quite a few boards we install heat sinks after CC and usually use an
>>epoxy to aid in heat transfer as well as loctite on the mounting screws.
>
> I
>
>>have been gigged for the residuals (just smears really) whether it is on
>>the solder pads or not. I know that we all are concerned with material
>>left over directly on the solder connections, but I am having trouble
>
> with
>
>>this one from a logical standpoint. I mean lets face it, you definitely
>>can't test for the presence of ionic contaminants or anything, but I know
>>the general impression is the boards should be clean.
>>
>>I know the simple answer here is to clean up all the residuals (and
>>everyone is instructed to do that), but there are times when stuff just
>>happens.
>>
>>Your thoughts
>>
>>Bruce Stilmack
>>GDLS-TO Manufacturing Engineer
>>(850) 574-4773
>>[log in to unmask]
>>
>>---------------------------------------------------
>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>>To unsubscribe, send a message to [log in to unmask] with following text in
>>the BODY (NOT the subject field): SIGNOFF Technet
>>To temporarily halt or (re-start) delivery of Technet send e-mail to
>>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>>To receive ONE mailing per day of all the posts: send e-mail to
>>[log in to unmask]: SET Technet Digest
>>Search the archives of previous posts at:
>
> http://listserv.ipc.org/archives
>
>>Please visit IPC web site
>
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
>
>>additional information, or contact Keach Sasamori at [log in to unmask] or
>>847-509-9700 ext.5315
>>-----------------------------------------------------
>>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|