TECHNET Archives

April 2002

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Mark Rusciolelli <[log in to unmask]>
Date:
Fri, 5 Apr 2002 08:23:45 -0500
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Mark Rusciolelli <[log in to unmask]>
Parts/Attachments:
text/plain (32 lines)
        I'm a little confused about gold plating as a solderable finish for circuit
boards and was wondering if anyone can clarify a few points.

        Most of our PCB's are have a hot air solder level finish, but finer pitches
and smaller parts are requiring us to look at boards with flatter surfaces
and it looks like Nickel-Gold finishes have become somewhat popular.

        From what I understand, gold can be applied electrolyticly, electroless
plating, or by immersion.  (I don't really understand the difference between
electroless and immersion).  Is any one method superior to the others?  It
seems like immersion leaves the thinnest amount of gold.  Does immersion
leave the flattest surface as well?

        Furthermore it appears that you can get hard and soft gold, at least with
an electrolytic process.  Is one better than the other?

        I appreciate any help.

Mark Rusciolelli
Nexus Custom Electronics

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2