TECHNET Archives

January 2002

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Date:
Thu, 31 Jan 2002 14:56:39 EST
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (50 lines)
Ed

In answer to your question, yes the benefit can be lost if the component is
cleaned.  We have worked with clients that have experienced problems with BGA
components that were balled using a low solids no clean flux. These units
were assembled with water-soluble solderpaste and cleaned in an aqueous
inline system.  The low solids no clean residue absorbed the activators and
moisture from the assembly process and created a corrosion cell on finished
assemblies.  I would recommend that good cleaning and drying process for the
components that will be subjected to aqueous cleaning of water-soluble
solderpaste.
We found that Ion Chromatography analysis corresponded well to the electrical
performance testing (failures had high chloride levels).



Terry Munson
CSL Inc.
P 765-457-8095
F 765-457-9033

<A HREF="www.Residues.com">www.Residues.com</A>



<<  have a client using our Reballing system to recondition all sorts of BGA
and uBGA for re-use after de-soldering. They are currently using a water
soluble paste and cleaning with DI, however the residual absorbed moisture
presents a concern, so the devices are baked after cleaning. This increases
turnaround time, so they are considering moving to a no-clean process.

 My opinion is that there will be residues and they could possibly be
incompatible with subsequent platforms utilized by the end user, as well as
creating aesthetic impact. Cleaning alternatives for no-clean fluxes rival
the more aggressive (therefore more forgiving) water solubles, so the benefit
is lost if cleaned.

Ed

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2