Yes this is a problem! One thing that can be done about it is to bake the dewar while pulling a vacuum on it or another is the use of ultraviolet light.(To dry it up) I don't know what else I can tell
you without revealing anything that is proprietary.
||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Dan Sadley
[log in to unmask]
Princeton Instruments,Inc.
3660 Quakerbridge rd.
Trenton, NJ 08619
(609) 587-9897 x-179
Fax (609) 587-1970
||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
----------
From: PC :[log in to unmask]
Sent: Wednesday, August 20, 1997 3:02 PM
To: [log in to unmask]
Subject: [TECHNET] Moisture in Liquid Nitrogen
<<File: ENVELOPE.TXT>>
Greetings:
I have a question regarding moisture in LN2 Dewars. My assumption is under
normal conditions, the moisture would be frozen solid and have a very low
vapor pressure, but what happens to the ice as the dewar becomes empty...
anyone else experienced a problem that could be attributed to moisture in a
LN2 system?
Thanks,
Tom Ostertag
[log in to unmask]
[log in to unmask]
[log in to unmask]
Minneapolis, MN
|
|
|