TECHNET Archives

July 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Mon, 12 Jul 1999 07:44:19 -0400
Reply-To:
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
Organization:
Photocircuits Corporation
From:
Will Miller <[log in to unmask]>
Parts/Attachments:
text/plain (16 lines)
All,
        For those of you using CIBA Probimer 77 solder mask, how has it been
running for you?
We have been testing the material for the past 6 months in a curtain coat
application and have seen many problems with the curtain's stability.  Has
anyone seen this issue?

        Thanks in advance in for your input.

Will Miller
Process Engineer, Glen Cove Mask Operations