It would not be at all unexpected to observe a higher relative
concentration of tin in an area determined to have a "thin" HAL deposit.
The XRF is responding to the ratio of tin to lead, and given you are
approaching the copper/solder interface, and more specifically the
tin/copper interface, it would be naturally preferential to tin
concentration.
Sounds like you are within expected conditions, other than the thin solder
deposits. May I assume they are on larger ground areas? There is a direct
correlation between deposit thickness and area size under given conditions
Hope this helps!
Joseph Webb
TET/Halco
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|