Hi Brian - you can get OFHC copper samples from Goodfellow
(www.goodfellow.com) or from any major metals distributor in your area.
Goodfellow will cost more but has a wide variety of forms/sizes, a metals
distributor will be cheap but there will be a minimum quantity buy
requirement plus you may only find rolled sheet stock available. Good luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
Christopher Jorgensen <[log in to unmask]> on 02/17/99 04:52:34
PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to Christopher Jorgensen <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] Copper Sample Supplier
I was wondering if you could provide a source where I can get copper
samples for
performing a solderability test. The samples don't necessarily need to be
oxygen
free, as we can bright dip finish them here. OSP coating is also not a
requirement.
I would appreciate any information you might have.
Thanks again,
Brian Looney
Manufacturing Engineer
Laughlin-Wilt Group
9825 SW Sunshine Ct
Beaverton, OR 97005
(503) 672-4370
fax: (503) 641-9145
email: [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|