Hi Dave,



Isn't it so-called "Nickel foot" you see on your boards?



Can you ask Steve to post pictures?



Regards,



Vladimir

------Original Message------

From: Dave Connitt

Sender: TechNet

To: [log in to unmask]

ReplyTo: TechNet E-Mail Forum

ReplyTo: [log in to unmask]

Sent: Mar 5, 2009 15:09

Subject: [TN] ENIG Question



Hello All,

I have a question regarding a strange situation regarding reflow

soldering ENIG finish boards.

We have seen a few boards that have what seems to be gold "washing "

down between pads and creating shorts. This seems to come and go. This

is a flex circuit that is placed on a pallet to go through our SMT line.

One other bothersome issue is that we are having difficulty getting

proper solder stencil alignment across all the flexes in the pallet. I

am pushing to have the flex "panelized" from the vendor to increase

positional accuracy but the jury is still out on that.

I suspect these two issues are related. If the solder gets deposited

"off pad"slightly could the washing process be moving some of the gold

in between pads? I attached an example.

Has anybody come across this?

If so, what was the solution?

 

Thanks,

Dave Connitt CID+



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------







SENTEC

11 Canadian Road, Unit 7.

Scarborough, ON M1R 5G1

Tel: (416) 899-1882

Fax: (905) 882-8812

www.sentec.ca


ATOM RSS1 RSS2