In a message dated 97-11-04 05:05:57 EST, you write:
> Can any one help me with a solution to this problem,
I'll give it a shot.
> we have recently experenced board failures because of a contamination
> across various sm capacitors which first looks like a splat of black
paint
> which run diagonally across the cap, under a microscope it looked like
> fern leaves.
The black material could be a number of things: dense dendritic growth,
carbonizing from an arc, leaking electrolytic solution from a cap, stray
encapsulant material, etc. If I could see it, I would have a better idea.
Any chance of making a digitized photo and sending me one? The "fern leaf"
structure indicates it is probably dendritic growth.
> Our boards are wave soldered and w edo not clean after solder flow.
What are you wave soldering with and are you mixing any flux technologies?
Doug Pauls
CSL
[log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|