text/plain (111 lines)
I  agree with Erik but at same time, it is discreation of sender .
Philips probably had not meant the diversion of information.
We look at technet as tool for spreading engineering. Many a times I do
also write my personal mail in case somebody want to contact me
directly. But intent is always same-info should always come through net
.
There is no need to worry about flood when we are facing scarcity of
relevant engineering information on current issues:BGAs, high density
packages,facilities requirements and new technologies such as Flip
chips, microBGAs, MCMs, DCAs and many more.
I had very poor response on some of the aforementioned
topics--facilities requirements and BGAs.I am thinking to post the
messages again.Where is flood???Please do encourage experts to flood the
technet and not to divert to other outletsinstead. We are more than 1300
now ,looking at this technet as problem solving tool.Keep it up and be
proud of it.
I hope many participants on Technet will agree with me.

thanks.


> ----------
> From:         Erik C. Olson[SMTP:[log in to unmask]]
> Sent:         October 14, 1997 4:59 PM
> To:   [log in to unmask]
> Subject:      Re: [TECHNET] X-Ray Inspection Equipment
>
> I disagree with Phillip.  Please do "flood the TechNet" since others
> of us
> may be interested in the information (like me).  Isn't that what the
> TechNet is for?
>
> Erik Olson
> Westell, Inc.
>
>
>
>
>
>
> [log in to unmask] on 10/14/97 03:58:39 PM
>
> Please respond to [log in to unmask]; Please respond to
>       [log in to unmask]
>
> To:   [log in to unmask]
> cc:    (bcc: Erik Olson/Westell/EIT)
> Subject:  [TECHNET] X-Ray Inspection Equipment
>
>
>
>
>         I would appreciate some information on  models of X-Ray
> Inspection
> Equipment
> that is being used to inspect Micro BGA solder connections.  My
> company has
> been building
> surface mount assemblies down to 15mil pitch for several years and is
> investigating Micro BGA
> devices for Flash Memory.
>         To keep from flooding the TechNet, responses may be directed
> to me
> at:
>                 [log in to unmask]
>         Any response will be appreciated.
>                                                 Thank you!
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV
> 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following
> text in the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ##############################################################
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV
> 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ##############################################################
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2