Mike: ED/Double treat may be the easiest Copper to bond to existant... in fact, some time it causes "lock-in", and the resist is VERY difficult to get off...so this may not be a real relevant test.
You run through Shadow... which has a microetch... what is your rinsing quality after microetch? Do you rinse in a tank, or spray?
One possibility..is the tarnishing of the boards.. they tarnish easily after microetch, unless the rinse is very well done... this means, if you rinse in a tank, you should never be in the tank more than 30 seconds.. and you should have a multi-tank cascade.
If spray, is the incoming fresh water going into the sump, or into the final spray bars?
The tarnish is triggered by dissolved Copper... and if you are not getting all of the Copper off, or (in a tank) staying in the presence of dissolved Copper too long... this could be causing Copper tarnish.
Rudy Sedlak
RD Chemical Company
Mike Wolf <[log in to unmask]> wrote:
We are experiencing resist adhesion failures in a random spotty nature,
after develop traces and or pads will just not be adhered.
We run a cert. piece everyday that never has these problems.
The cert piece is ED/double treat right out of the box.
The copper that has the adhesion problems has been processed in our
shop, we run electrochem's shadow system.
I know its not much to go on more details available to anyone
interested.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------
Do you Yahoo!?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
Win 1 of 4,000 free domain names from Yahoo! Enter now.
|
|
|