TECHNET Archives

June 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Tempea, Ioan" <[log in to unmask]>
Date:
Tue, 26 Jun 2007 08:12:07 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Rueda, Ernesto" <[log in to unmask]>
Subject:
From:
"Rueda, Ernesto" <[log in to unmask]>
Content-Type:
text/plain; charset="US-ASCII"
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
MIME-Version:
1.0
Parts/Attachments:
text/plain (77 lines)
Try to ask Fuji regarding their "test boards". I work
Hi Ioan,



Try to ask Fuji regarding their "test boards". I worked in a company

before and we have Fuji CP6 and IP2/3. We used their test board for

placement test/calibration.



Regards,



Ernesto V. Rueda

 



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan

Sent: Tuesday, June 26, 2007 6:56 AM

To: [log in to unmask]

Subject: [TN] SMT placement test PCB



Dear colleagues,



I am pondering the necessity of having a custom PCB designed, PCB that

would serve for periodical testing of the placement of our machines. We

have Fuji CP6 and IP3, just FYI as I don't think the board should be

speciffic to a machine in particular.



I am wondering if any of you felt the need of having a special PCB to

perform this, or you find the glass board for IP and the regular Fuji

test board sufficient?



I have checked the available boards from Practical and Topline and find

them unsatisfactory when it gets to 0402 and 0201 landpatterns.



If you would order a special PCB, how would you use it? What components

should it be there?



Thanks,



Ioan



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0 To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to [log in to unmask]: SET

Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the

posts: send e-mail to [log in to unmask]: SET Technet Digest Search the

archives of previous posts at: http://listserv.ipc.org/archives Please

visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------

Confidentiality Notice:

The information contained in this transmission is legally
privileged and confidential, intended only for the use of the
individual(s) or entities named above. This email and any files
transmitted with it are the property of Pelco. If the reader of
this message is not the intended recipient, or an employee or agent
responsible for delivering this message to the intended recipient,
you are hereby notified that any review, disclosure, copying,
distribution, retention, or any action taken or omitted to be taken
in reliance on it is prohibited and may be unlawful. If you receive
this communication in error, please notify us immediately by
telephone call to +1-559-292-1981 or forward the e-mail to
[log in to unmask] and then permanently delete the e-mail and
destroy all soft and hard copies of the message and any
attachments. Thank you for your cooperation.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2