TECHNET Archives

January 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vnSHA-0000XTC; Thu, 23 Jan 97 10:45 CST
Content-Type:
text/plain; charset=US-ASCII
Old-Return-Path:
Date:
Thu, 23 Jan 1997 11:53:37 EST
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
Content-Transfer-Encoding:
7bit
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/9535
From [log in to unmask] Thu Jan 23 14:
34:56 1997
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"6l2Nu1.0.ZnI.SMvvo"@ipc>
Subject:
From:
X-Status:
X-Loop:
MIME-Version:
1.0
Message-Id:
Parts/Attachments:
text/plain (38 lines)

    \0
   TO:         I4235700 IBMMAIL   new address for ipc technet 25.6.96

   FROM:       DSTEWART EX2       D.Stewart        - Product Development Manager.

   DATE:       23 January 1997
   SUBJECT:    RE: REVERSE PULSE PLATING SYSTEM

    Without doing any advertising, because Exacta "stuck with" the
    two guys who believed in pulse plating and designed the pulse
    "engine", and helped them convince their new employer that they had
    a product, we installed pulse on our two main plating lines in 1995
    having previously used it for 6 years on our handlines. A number of
    other UK sites have also installed it, as have two big players in
    Germany and Holland. I think that we all agree that the system
    gives enough benefit to justify the investment.
    Perhaps the reason that you thought it had died was because all the
    development was done in the "l'il ole UK" where we don't have any
    innovation worth pursuing (sic).
    Anyhow, if you do want any information on Pulse plating of acid
    copper contact Chemring on +44 1705 735457

    Dougal
    Exacta

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2