Mike Bailey is right on the money.
Most Permanganate baths will tarnish hell out of the Copper, but not dissolve
any significant amount of Copper, as they are typically little more than
Caustic and Permanganate. However, the neutralizer bath, depending on various
factors, like type of chemistry, and age, etc. can do a nice number on the
Copper.
Rudy Sedlak
RD Chemical Company
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|