Kaye,
It all depends on the size of leads and how many cracked solder joints you
can stand. There are commercially available alloys that are nearly crack
free and others that have lots that do indeed propagate during thermal
cycling.
John Maxwell
At 10:19 AM 5/10/2005, you wrote:
>Technet,
>
>Can anyone share what the differences are between
>Tin-Silver-Copper (SAC) solder and the Tin-Copper-Nickle solder
>(or ultimately, the solder joints) for use in wave solder machines?
>Why would someone want to use one over the other?
>
>Thanks,
>
>Kaye
>
>
>
>
>
>
>
>
>
>
>
>
>
>
>CONFIDENTIALITY NOTE: This message is intended only for the use of the
>individual or entity to which it is addressed and may contain information
>that is privileged, confidential, and exempt from disclosure under
>applicable law. If the reader of this notice is not the intended
>recipient, you are hereby notified that any dissemination, distribution or
>copying of this communication is strictly prohibited. If you have received
>this communication in error, please notify the sender immediately.
>
>
>
>_____________________________________________________________________________
>Scanned by IBM Email Security Management Services powered by MessageLabs.
>For more information please visit http://www.ers.ibm.com
>_____________________________________________________________________________
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>
>--
>No virus found in this incoming message.
>Checked by AVG Anti-Virus.
>Version: 7.0.308 / Virus Database: 266.11.5 - Release Date: 5/4/2005
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|