TECHNET Archives

December 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Hiteshew, Michael" <[log in to unmask]>
Date:
Mon, 6 Dec 1999 06:36:48 -0600
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Kelly M. Schriver" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Kelly M. Schriver" <[log in to unmask]>
Parts/Attachments:
text/plain (96 lines)
Michael -

I think what Doug is trying to point out is that the requirement for fungus
resistance is already posted in the laminate material specification in most
cases (ref. IPC-4101 table 5) as a part of the basic resin system
qualification.  Accordingly, an additional requirement stipulated in the
purchase order would not be required, and may only cloud the issue by
imposition of additional specifications.

Regards - Kelly
-----Original Message-----
From: Hiteshew, Michael <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Friday, December 03, 1999 4:42 PM
Subject: Re: [TN] Fungicidal Laminate


Hi Doug,
        We've been discussing this same issue here at Lockheed. According to
IPC-6012 (Qualification and Performance Specification for Rigid Printed
Boards) - Section 3.11 (p17), "Special Requirements", reads in part:
        "When specified on the procurement documentation, some or all of the
special requirements listed in the following paragraphs shall apply. ...".
Section 3.11.3, which follows this statement, covers fungus resistance.
Notice the key words "When specified..". This qualifying comment occurs
again in Appendix A (p27). In addition, MIL-HDBK-454, Section 4.4, "Fungus
Testing", reads in part:
        "Group II materials should be subjected to the fungus test specified
in MIL-STD-810...". Under Group II materials are epoxy glass-fiber laminates
and epoxy resin. Also listed is polyurethane, the main component in Type UR
conformal coating. Type AR (acrylic) is listed as a Group I (fungus inert)
material.
        So it sounds like these organic materials are fungus nutrients and,
depending on your application environment, may need to treated with
fungicide. Since this is a special requirement, it will need to specified on
the procurement documentation.

Michael Hiteshew
Lockheed Martin Launching Systems
[log in to unmask]
(410) 682-1259


> ----------
> From:         Douglas O. Pauls[SMTP:[log in to unmask]]
> Reply To:     TechNet E-Mail Forum.;[log in to unmask]
> Sent:         Friday, December 03, 1999 7:34 AM
> To:   [log in to unmask]
> Subject:      Re: [TN] Fungicidal Laminate
>
> In a message dated 12/02/1999 2:54:44 PM US Eastern Standard Time,
> [log in to unmask] writes:
>
> >
> >  It seems to be my week for strange requests.
> >  Does anyone know of a fungicidally treated FR4 laminate? Or of any
> >  fungicidal treatment which can be applied to an assembled circuit
> board.
> >
>
> I can't really see the need for a fungicide.  Most IPC specs have the
> requirement that the base material, such as laminate, mask, and coating be
> non-nutrient in nature, which means it would not support growth of a
> fungus.
>
> Doug Pauls - CSL

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2