TECHNET Archives

April 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 19 Apr 2005 13:27:51 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, John Parsons <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
From:
John Parsons <[log in to unmask]>
Parts/Attachments:
text/plain (32 lines)
We have sent a board to our off-shore vendor for fabrication.  The pcb
finish is spec'd as immersion gold with selective hard gold.  Our Chinese
vendor has come back asking if they can process as flash gold with selective
hard gold.



Correct me if I am wrong as I have seen "flash gold" and "immersion gold"
referenced as the same process but I believe that flash gold is an
electrolytic process is it not?  I am leaning towards approving this request
but is there anything I should be aware of or question before I do so?  Any
"gotchas"?  From what I have read "flash" gold can be process as either hard
or soft.  Can I assume that if they are going to use it to replace immersion
gold that the finish will be comparable for solderability?



John Parsons




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2