TECHNET Archives

October 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Date:
Tue, 16 Oct 2012 14:10:56 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Message-ID:
Subject:
From:
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (118 lines)
That shows you have a real steak in the game.
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
Sent: Tuesday, October 16, 2012 4:59 AM
To: [log in to unmask]
Subject: Re: [TN] board baking - thread continuation

Buy a meat vacuum seal less than 50 dollars. 
--------------------------
Sent using BlackBerry


----- Original Message -----
From: Robert Kondner [mailto:[log in to unmask]]
Sent: Monday, October 15, 2012 10:33 PM
To: [log in to unmask] <[log in to unmask]>
Subject: Re: [TN] board baking - thread continuation

Bev,

  I was just wondering if a tape seal is completely ineffective and if there
is any value with such a quick low cost closing scheme.  

 I ordered some bags, desiccants and moisture indicators, I will play around
with them some. 

Thanks,
Bob

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Monday, October 15, 2012 7:51 PM
To: [log in to unmask]
Subject: Re: [TN] board baking - thread continuation

Bob,
I don't know how they compare, mainly because you don't say how big of a
surface area and the length of the incomplete seal and also the fact that I
can't do the math anyways.  :(

But unless one is talking about real moisture barrier bags that are totally
sealed, then you are just talking about "short term" protection anyways. ALL
plastics let water diffuse.  Non-porous aluminum doesn't, unless it corrodes
through.

Bev

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Kondner
Sent: Monday, October 15, 2012 11:35 AM
To: [log in to unmask]
Subject: Re: [TN] board baking - thread continuation

Hi,

 According to content on some sites simple taping might be OK and heat seal
not required. 

I wonder how moisture diffusion through an incomplete tape seal and a bend
compares to bag surface diffusion.  

Bob K.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Glen Herzog
Sent: Monday, October 15, 2012 12:10 AM
To: [log in to unmask]
Subject: Re: [TN] board baking - thread continuation

Joyce Koo recommended a dry box.  I agree that that is recommended,
especially for short term use such as you've used some of the components and
you will use the rest in a few days to a few weeks.  However, if you need
longer term storage I recommend purchasing moisture barrier bags, desiccant
and moisture indicator cards.  They're relatively inexpensive.  You would
need a heat sealer ($200-$300 and simple to use) I would not worry about
vacuuming the bag, it's probably not worth the effort.  The formula for how
much desiccant to use depends on what desiccant is used.  For example you
might take  look at: 
http://texastechnologies.com/moisture-control/desiccant/silica-gel/packaged/
sorb-it-silica-gel-unit-size.htm
for one example.  I have no investment in that company, it's just a
reference to an example.

Good luck


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2