Jonathan,
      The predominant composition of any reduced oxide should be a mixture
of copper metal, cuprous chloride, and cupric chloride, mostly cuprous.
However, after some time has passed, and the circuit has gone through
thermal excursions, much of this will have re-oxidized back to cupric
chloride.  Any organic found would be only a residual from processing.  Of
course, any object that has been exposed to earth's atmosphere will have
carbon and oxygen adsorbed on it's surface, so the presence of C and O by
Auger is probably not a significant find.

Regards,

Denis Morrissey




             Jonathan.A.Noquil
             @FAIRCHILDSEMI.CO
             M                                                          To
             Sent by: TechNet          [log in to unmask]
             <[log in to unmask]>                                          cc

                                                                   Subject
             03/07/2003 12:10          [TN] Black Oxide
             AM


             Please respond to
              "TechNet E-Mail
                  Forum."
             <[log in to unmask]>
             ; Please respond
                    to
             Jonathan.A.Noquil
             @FAIRCHILDSEMI.CO
                     M







Hello Guys:
I would like to ask you regarding my analysis.
I examined a competitor package that passed MSL1 criteria.
We found out that the surface of the package is black (improved EMC
adhesion),
and i suspect that it was black oxide. Is there any analysis method to
confirm this?
We did Auger analysis and found these Eleements (Carbon and Oxygen), I
would like to ask if
black oxidation contains carbon?
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

regards

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2