TECHNET Archives

July 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
James Patten <[log in to unmask]>
Date:
Wed, 22 Jul 1998 07:55:32 -0700
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="ISO-8859-1"; Name="Message Body"
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, James Patten <[log in to unmask]>
Parts/Attachments:
Message Body (21 lines)
  REGARDING           ASSY:Reliability, SMT

With regards to surfmnt glass diodes (melf-type), how does one protect the body
from conformal coating. In the past, we sleeved the axial body to protect it from
CTE mismatch. I haven't yet contacted Mfg about the exact P/N of the conformal
coat material. Is this necessarily the reason for crack initiation? Could the cause be
the 'cooling' slope during reflow, thereby allowing the coating mismatch to
propogate the cracking?

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2