TECHNET Archives

May 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Hernefjord Ingemar <[log in to unmask]>
Date:
Tue, 29 May 2007 13:52:01 -0500
MIME-version:
1.0
Reply-To:
Content-type:
text/plain; charset=us-ascii
Subject:
From:
Kathy Kuhlow <[log in to unmask]>
In-Reply-To:
Organization:
Teleflex Mail
Content-transfer-encoding:
7BIT
Parts/Attachments:
text/plain (147 lines)
Inge, 

When NAFTA first came into play, the company I worked for ran to the border
for cheaper products to be built. We built industrial computing products at
the time so it needed to be pretty durable. We ended up within 9 months
scrapping everything built south of the border due to two reasons. One was a
dendrite growth on all of the gold (simm sockets mainly) due to water
quality (said it was DI but apparently our definitions of DI differed a
bit). The second reason was flux under the older 386 and 486 chip sets.
There was flux underneath that never was cleaned up. We found that the flux
was eating through the traces underneath the chips. I suspect it was due to
a solder issue and the boards were flooded for rework but insufficiently
cleaned up. About 2000 boards were scrapped because it was impossible to
determine the extent of both problems. Left south of the border shortly
after that and only used them for cables afterwards. 

Kat

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: Wednesday, May 23, 2007 3:11 AM
To: [log in to unmask]
Subject: Re: [TN] Flux residue, burnt flux

What I say now may cause some to think that I'm member of Ku-Flux-Klan,
which is not the case. So, we follow the general habit of removing 'all'
flux residues. However, I can't deny, that I think this flux removal
hysteria is little exaggerated. I've been in the business for so long a
time, and I have not seen many reported failures that have been caused
by flux residues. In theory, flux residues have many ingredients that
can cause corrosion, leakage current, decreased insulation etc, but it
seems as that does not happen in reality. 100% cleanliness is satifying
and beautiful, but costs a lot to obtain.
Just a thought. Would be very interesting if anyone could describe a
case with flux residues causing massive failures.
Inge 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
Sent: den 23 maj 2007 09:38
To: [log in to unmask]
Subject: Re: [TN] Flux residue, burnt flux

I'm sure that an eminent co-contributor to this forum will tell you, "it
depends". If the flux is truly burnt, i.e., black, this indicates
pyrolysis, which is a fancy word meaning decomposed by heat. Pyrolysis
indicates that the residues have split apart into numerous compounds,
leaving carbon-rich stuff. Elemental carbon can be an electrical
conductor; do you want conducting particles in your assembly? They may
appear fixed in place now, but will they remain so during the life of
the equipment?

More important, WHY are they there? It may be because the operators
don't keep the bits of their irons clean. Do they wipe them on a wet
sponge before each joint is made? It may be that the time/temperature
conditions of the joint being made are far from optimal. It may be lack
of adequate training of the operators. I can't tell. Whatever,
prevention is better than cure; a lttle research into the causes may
give you the answer.

As to flux flow, maybe your solder wire simply has too much flux. Some
manufacturers allow you to choose the percentage. Yes, it is easier to
solder with an excess. It's a compromise.

What you have not told us is the essential information: what kind of
assemblies are you making. You can obviously be more tolerant of
imperfections if you are making toys than if you are making inertial
guidance or satellite systems. Probably you are somewhere between thes
extremes. "It depends"!

Brian

Sue Powers-hartman wrote:
> We fight a constant battle with operators leaving burnt flux in 
> joints. Maybe only a small speck, but drives the inspectors nuts.  The

> way I read JStd-001D, if they can not see it at referee inspection
power, they have to accept it.
> How dangerous is this burnt flux to the PWB?  If it's not seen at 
> inspection power and left on the board, what happens.  Also, what
about no clean flux?
> Our solder training video says that if no clean flux runs out to far 
> and is not heat activated, it can cause problems. Operators watch this

> video, but somehow do not get this. They say that it's no clean, they
can leave it all on.
> I keep saying that this can be a problem, and then they ask me, how 
> far out can the flux be away from the joint before it's unacceptable.
> 
> Wow, I'm glad I found this forum, I have so many questions to ask you
guys.  
> Anyway, thanks for the help on this subject.
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
> unsubscribe, send a message to [log in to unmask] with following text in

> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET

> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the 
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the 
> archives of previous posts at: http://listserv.ipc.org/archives Please

> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at 
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2