TECHNET Archives

February 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Adam Seychell <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Adam Seychell <[log in to unmask]>
Date:
Fri, 29 Feb 2008 22:02:31 +1100
Content-Type:
text/plain
Parts/Attachments:
text/plain (29 lines)
Hi all.
I'm trying to solve a problem of pitting around the holes after 
ammoniacal etching. I suspect my problem is insufficient deposits of 
electroplated tin resist around the holes, which is making it more 
susceptible to attack by the etchant. The reason I think its a tin 
problem is because prior to etching, the tin deposits appear solid and 
smooth when viewed under a microscope. However after etching there is 
evidence of pitting around many holes.
The problem seems to go away with excessive plating, about 8um or more. 
Normally I've not had a problem at only 2~3um.

Also is it normal to have a small amount of white foaming hydrogen gas 
above the PCB while tin plating ? The tin bath is an acid stannous 
sulfate type with brighteners, and has always been a milky yellow 
appearance.


Adam Seychell

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2