Wow, now that is something new. Doing what we do, we get quite a few
customer driven QA audits and strangely, every single one has something
different to point out as an "observation". Never a show stopper but always
something. I have yet to have anyone say anything about the fans though.
Lloyd Duso
Diamond-MT
Plant Manager
(814) 535-3505
www.Diamond-mt.com
On Wed, Jun 1, 2016 at 10:14 AM, Douglas Pauls <
[log in to unmask]> wrote:
> Good morning all,
>
> We had an outside audit "observation" that I would like some outside
> opinions on. In your facilities, are simple air circulation fans, usually
> plastic blades and a plastic housing (think inexpensive Walmart) targeted
> as an ESD generator? I have never heard of such and my view is that if our
> humidity stays above the 30% minimum found in most ESD standards, then we
> should not have charge generation.
>
> So, are cheapy plastic fans an ESD hazard?
>
> Doug Pauls
> Principal Materials and Process Engineer
> Rockwell Collins
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|