TECHNET Archives

January 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Phil Hersey <[log in to unmask]>
Date:
Wed, 27 Jan 1999 16:28:21 -0800
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
Phil Hersey <[log in to unmask]>
Parts/Attachments:
text/plain (25 lines)
I just found out that I can replace a $120 LTCC substrate with a $1.95
microvia PCB.  Trouble is the PCB comes with nickel/flash gold so cannot be
wire bonded using our gold ball bonding equipment.  Evidently it can be
bonded using ultrasonic aluminum wedge.  This MCM has over 700 wires in a
1.5"x1.5" area (one of the ASIC's has 220 wires itself)- military
application.

Does anyone have experience with al. wedge on such boards?  Construction is
175C Tg FR4 core with 3 layers of photovia on top (photoimageable epoxy
plated up with copper).  Will it work?  Who makes the best bonder?

Phil Hersey, Hytek Microsystems

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2