TECHNET Archives

September 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 17 Sep 2009 08:53:55 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Dave Schaefer <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Type:
text/plain; charset="ISO-8859-1"
Content-Transfer-Encoding:
quoted-printable
From:
Dave Schaefer <[log in to unmask]>
Parts/Attachments:
text/plain (26 lines)
Toby,

For HDI designs (via in pad) I pour ground underneath BGAs and ensure that
any connections to the BGA ball are thermals. This eliminates soldermask
defined land areas which are problematic during manufacture.

For most non-HDI designs your observation is correct - there's not likely a
lot of pour under the BGA anyways, so not much point in having it there, and
I'll normally block out the area if pouring on the surface. I do normally
employ a stackup where the adjacent layer (t-1, b-1) is a plane in these
situations. The one reason I would consider keeping the pour under the BGA
is if it is large enough (and required) to provide some thermal benefit.

Hth,
Dave

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2