TECHNET Archives

February 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Tony Steinke <[log in to unmask]>
Reply To:
Tony Steinke <[log in to unmask]>
Date:
Fri, 16 Feb 2001 16:00:20 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (64 lines)
Bob,
This reply is probably a few weeks old but here it goes anyway.
The flaking resist you are referring to I am assuming is resist breakdown.
I would look more at your preclean and lamination operations.
Things to look into:
1. Etch rate or concentration of preclean solution. Also check rinse nozzles
and if
you do not have filtration on your rinse I would recommend it.
2. Check exit temperature of panels being laminated. Even though your
temperature of
rollers may be in spec. if boards are being laminated at a fast linespeed
this would greatly
affect your adhesion.
3. Profile your laminating rollers with infrared thermometer. (Grainger
carries a very nice compact one for $100.00.) Also check the footprint of
your laminating rollers- you could have uneven
pressure.
Hope this helps
Take care
Tony Steinke
----- Original Message -----
From: Robert Lazzara <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, February 12, 2001 1:36 PM
Subject: [TN] DRY FILM BLUES


> Dear PWB 'Netters:
>
> We're trying to tweak our yields at Dry Film (plating resist). Our pareto
> shows cracked, flaking resist as the next item on the hit list. The
condition
> is not unique to high current density areas, traces, etc..
>
> Any thoughts are appreciated.
>
> Robert Lazzara
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2