TECHNET Archives

June 2003

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Cagle, James" <[log in to unmask]>
Date:
Thu, 12 Jun 2003 17:14:09 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Morse, Carrie" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Morse, Carrie" <[log in to unmask]>
Parts/Attachments:
text/plain (145 lines)
We have a closed loop system and have not had much luck with the Water Soluble.
From a cost standpoint, and additional DI tank is needed and that one as well
as the others will need to be changed more frequently.  

In addition, we are limited to using a mask developed by our closed loop
filtration supplier.  If we use anything else, they will not accept
responsibility for damage to the tanks.



-Carrie

-----Original Message-----
From: Cagle, James [mailto:[log in to unmask]]
Sent: Thursday, June 12, 2003 5:04 PM
To: [log in to unmask]
Subject: Re: [TN] evaluation of peelable solder mask for wave solder


I like the water-soluble masking. I have used in a open loop system. You
have to be carefull what you use in a closed loop system as it may ruin your
DI tanks. When using peelable, it loves to stay in small holes and star
washers. It is also eaiser to get off if a little thicker than too thin.
>
>                                  James Cagle
> Tyco Printed Circuit Group-Hayward Division
>                       email: [log in to unmask]
>


-----Original Message-----
From: Barmuta, Mike [mailto:[log in to unmask]]
Sent: Thursday, June 12, 2003 1:39 PM
To: [log in to unmask]
Subject: Re: [TN] evaluation of peelable solder mask for wave solder


In addition to the great list Carrie provided,  you may want to consider the
following:

*       Ease of removal for various features and configurations of
application
*       Resistance to breakdown in the flux and solderwave
*       Ionic characteristics of the mask
*       Compatibility with board and final finish materials
*       Applied shelf life
*       dispensable Vs screenable

If you are post wavesolder washing the boards have you considered a soluble
mask instead of peelable which can be difficult and time consuming to
remove?

Regards

Michael Barmuta

Staff Engineer

Fluke Corp.

Everett WA

425-446-6076




-----Original Message-----
From: Tenison Stone [mailto:[log in to unmask]]
Sent: Thursday, June 12, 2003 12:10 PM
To: [log in to unmask]
Subject: [TN] evaluation of peelable solder mask for wave solder



Hi everyone,

I am working on a plan to evaluate peelable solder masks for wave soldering.


We currently use a latex that takes overnight to dry.  I have several
samples from different vendors to use in an experiment.

What parameters should be included in the experiment to ensure I make the
best decision for my process?

Thank you for your help.

Tenison Stone
Manufacturing Engineer
Telex Communications
1930 West First Street
Blue Earth, MN  56013
507-526-3205   x2164
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
507-526-3059 (fax)

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2