You might want to add a little about gold plating. Gold in itself does
NOT bond to solder. It does, however, protect against oxidation. The
gold plating has to be very thin, on the order of 2 - 3 micros. The
solder actually goes through the gold to bond to the surface underneath.
If the gold layer is too thick, the components will just fall off. We
had a board house plate the pads with a thicker layer used with edge
connectors, and most of the components just fell off. You have to be
very careful with the process.
Art
> -----Original Message-----
> From: Albert Mok [SMTP:[log in to unmask]]
> Sent: Wednesday, April 28, 1999 7:40 AM
> To: [log in to unmask]
> Subject: Re: [TN] Flash Gold??
>
> Dear technetters,
>
> We regard "flash gold"for gold thickness up to 2 microinch. The
> purpose of
> gold flash is to give protection of nickel against oxidation and also
> provide better solderability when compared with bare nickel. Flasg
> gold is
> very common for COB boards and the whole board will be electroplated
> for
> maximum 2 microinch.
>
> _____________________________________________________________
>
>
> At 06:58 AM 1999/4/27 -0700, David McCann wrote:
> >We have used flash gold on rigid flex products to maintain a
> solderable
> >surface. Typically I have seen approximately 4 microinches of Au (ie
> flash
> >Au referring to a very thin electroless plating), over 100
> microinches
> >minimum of electroless Ni over Cu.
> >
> >Regards,
> >
> >-----Original Message-----
> >From: TechNet [mailto:[log in to unmask]]On Behalf Of Nick Liang
> >Sent: Monday, April 26, 1999 11:41 PM
> >To: [log in to unmask]
> >Subject: [TN] Flash Gold??
> >
> >
> >All:
> >What is Flash Gold Process??
> >
> >Thanks for your answers.
> >
> >-----------------------------------------------
> >Nick Liang
> >QE Engineer
> >Quality Assurance Division
> >Gold Circuit Electronics Ltd.
> >Tel : (886) 03-4612541 Ext 417
> >Fax: (886) 03-4522094
> >Cell: (886) 0935-917151
> >E-Mail : [log in to unmask]
> >------------------------------------------------
> >
> >################################################################
> >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> >################################################################
> >To subscribe/unsubscribe, send a message to [log in to unmask] with
> following
> >text in the body:
> >To subscribe: SUBSCRIBE TechNet <your full name>
> >To unsubscribe: SIGNOFF TechNet
> >################################################################
> >Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section
> >for additional information.
> >For technical support contact Hugo Scaramuzza at [log in to unmask] or
> >847-509-9700 ext.312
> >################################################################
> >
> >################################################################
> >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> >################################################################
> >To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> >To subscribe: SUBSCRIBE TechNet <your full name>
> >To unsubscribe: SIGNOFF TechNet
> >################################################################
> >Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> >For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> >################################################################
> >
> >
> >
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|