TECHNET Archives

October 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TECHNET EMAIL FORMUM <[log in to unmask]>
Date:
Thu, 5 Oct 2006 08:34:23 -0500
Reply-To:
Subject:
From:
Gloria Brown <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Organization:
Burton Industries, Inc.
MIME-Version:
1.0
Parts/Attachments:
text/plain (40 lines)
Good Morning,

 

I need some information if available.  I am finding on our lead free solder
irons that there is a black substance that is rising up the soldering shaft.
We are currently using an Aim 270WR flux, SN100C LF Solder, LF tinner,
Solder iron temp is 720, they are WD1 solder irons.  

 

Can anyone give me some information on what this black substance may be?

 

Thanks

 

Gloria 

phone 906-932-5970  ext. 26

fax  906-932-9822

[log in to unmask]

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2