TECHNET Archives

January 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Graham Naisbitt <[log in to unmask]>
Date:
Wed, 28 Jan 1998 18:03:53 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Karen Tellefsen <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=ISO-8859-1
From:
Karen Tellefsen <[log in to unmask]>
Parts/Attachments:
text/plain (82 lines)
>
> I was a little bemused to receive Jerry's comment and have re-read my
> posting.
>
> Perhaps I should have worded it more clearly, particularly in view of
> Karen's reply. As I conduct this correspondence late in the evening, so
my
> communications are sometimes not as I would intend

Maybe Jerry was playing internet in the late evening, also.

> of course RF
> circuits use AC not DC and that the real issue with flux residues will be
> dielectric influences.

I would think so.

>
> I do not agree that AC will not cause dendrites. You have gazillions of
> reverse biasing going on at any moment which will certainly limit the
> ability of dendrites to form but over time they surely will, particularly
if
> there is something present to help them.

I am very doubtful that purely AC voltage will allow electrochemical
migration.
However, I am willing to change my opinion if decent experimental proof
is given.  AC on top of appropriate DC may indeed allow electrochemical
migration and dendrite formation to occur.  I also doubt that there would
be a
synergy of AC and DC combined, I would guess that the DC voltage will grow
dendrites like the AC voltage wasn't there.
>
> Many examples of RF circuitry that I have seen, are incorporated near to
DC
> inputs and other DC circuitry.

Such as power inputs for IC's etc., which are prime sites for
electrochemical
migration to occur.

> I am not sure how or why, one would
> selectively leave solder residues on an RF circuit where they would
> certainly compromise performance and not on the other areas (if present)
> where dendrites will form more readily.

Gloppy RMA residues (like good old Reliacore 15 (if Graham can do it, so
can I))
are not particularly "dendro-genic", nor do they degrade DC and low
frequency SIR,
like certain no-clean, organic-acid-type residues.  They tend to be
hydrophobic and
act like quasi conformal coatings.  However, their residues have dielectric
properties
that may have a deleterious affect on RF circuits.  Adding another layer of
dielectric
material near a stripline, resonator, etc., may mess up its designed
function.

>
> As to the application of SIR testing, we are looking at developing the
> measurement aspects of our system to include for AC circuitry testing
which
> Karen asked about in an earlier posting.
>

AC measurements could be a very interesting way of studying SIR and
electrochemical reactions in the thin moisture film on circuit board with
hygroscopic residues at high humidities.

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2