Juan,
I want to echo what Brian as said and add one thing.
In the United States the FAA and the DoD do not look favorably on the
"no-clean" process in general and conformal coating over "no-clean" fluxes
in particular for flight and mission critical systems.
David A. Douthit
Manager
LoCan LLC
"Juan T. Marugán" wrote:
> Hi technetters !
>
> Although I’ve read some messages about this matter, let me ask you some
> additional information.
>
> For our class 3 boards (avionics & military), we used rosin fluxes (ROL0).
> Now, we are thinking about to subcontract the assembly of some type of
> boards. One of the possible subcontractors uses no-clean organic flux
> (ORL0) for wave soldering. No post-solder cleaning is performed.
>
> After this assembly, we have to solder some components/wires to these
> boards so we will use our rosin flux. And, at the end, boards will
> conformal coated with Humiseal (acrylic).
>
> My questions are:
>
> 1.- Can the use of an organic flux (residues) to produce some effect in the
> solder joints performed later using rosin flux?
> 2.- What happen when these boards are cleaned with CFC solvents (Forane)?
> 3.- Have no-clean flux residues some effect in the quality (adherence, ...)
> of conformal coating?
>
> Thank you from Spain for your help.
>
> Juan T. Marugán López
> Production Quality Assurance
>
> INDRA EWS, Sociedad Anónima
> C/ Joaquín Rodrigo 11
> 28300 Aranjuez - Madrid (SPAIN)
> [log in to unmask]
> www.indra.es
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|