30 deg is very standard in the scoring industry. The larger the angle the
more edge distance you will need.
Please update your contact for Jim Mahoney
[log in to unmask]
Thank you,
Jim Mahoney
Quick Turn Flex Circuits, LLC
Applications Project Manager
P# 603-821-6571
F# 603-821-5723
M# 603-305-6250
** This email and all attachments have been scanned prior to being sent**
Confidentiality Notice: This page and any accompanying documents contain
information that is confidential, privileged or exempt from disclosure and
is intended for the exclusive use of the addressee. If you are not the
intended recipient, you are hereby notified that any disclosure, copying,
distribution or use of the contents of this information in any manner is
strictly prohibited.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Chandler
Sent: Wednesday, March 04, 2009 2:58 PM
To: [log in to unmask]
Subject: [TN] V-Score Standards?
Are there any industry standards for the angle of the V-score? Our equipment
supplier suggests 30 deg. but some of our PCB suppliers say they don't have
30 deg blades.
Thanks in advance,
Brian
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|