TECHNET Archives

May 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 29 May 2007 14:11:02 -0400
MIME-version:
1.0
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Jones, Evamaria" <[log in to unmask]>
Subject:
From:
"Jones, Evamaria" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (561 lines)
Sorry technetters...


 


Eli,





For class 2 product, you need at least 180 degrees of circumferential wetting , observable in the hole, on the primary side. That solder, if properly wetted,  bonds the lead to the to the barrel in a supported hole confiquration. Note picture 7-115 on page 7-54 that shows 100% fill but a black ring around the lead. Just because you have solder present doesn't mean it is wetted or bonding the component to PTH barrel. That condition is a defect; because, it doesn't meet the 180 degrees wetting on lead or barrel.  The solder didn't bond to the finish on the lead (usually solderability, improper dwell, or thermal relief issues/heat sinking). Occasionally you will see that ring around the barrel...same defect...the solder didn't  bond/wet to barrel.





Since you only need 75% fill or the exception of 50% fill for thermal planes, no solder is required to be present on primary side pad.








 


Evamaria Jones 


Quality Assurance Specialist


Electronic Manufacturing Skills Instructor


General Dynamics Information Technology


(703) 874-6796 direct 


(540) 522-8823 cell


[log in to unmask]


www.gdit.com <https://owandhm.gd-ns.com/exchweb/bin/redir.asp?URL=http://www.gdit.com/> 





________________________________





From: TechNet on behalf of Jones, Evamaria


Sent: Tue 5/29/2007 1:38 PM


To: [log in to unmask]


Subject: Re: [TN] Fw: Status of IPC Solder Inspection Criteria

















Evamaria Jones


Quality Assurance Specialist


Electronic Manufacturing Skills Instructor


General Dynamics Information Technology


(703) 874-6796 direct


(540) 522-8823 cell


[log in to unmask]


www.gdit.com <https://owandhm.gd-ns.com/exchweb/bin/redir.asp?URL=http://www.gdit.com/>





________________________________





From: [log in to unmask] [mailto:[log in to unmask]]


Sent: Tue 5/29/2007 12:53 PM


To: [log in to unmask]; Jones, Evamaria


Subject: RE: [TN] Fw: Status of IPC Solder Inspection Criteria











Hole fill is 50% for Power/Grounds and 75% for signals.





-----Original Message-----


From: TechNet [mailto:[log in to unmask]] On Behalf Of Jones, Evamaria


Sent: Tuesday, May 29, 2007 8:26 AM


To: [log in to unmask]


Subject: Re: [TN] Fw: Status of IPC Solder Inspection Criteria





What IPC class?





Evamaria Jones


Quality Assurance Specialist


Electronic Manufacturing Skills Instructor


General Dynamics Information Technology


(703) 874-6796 direct


(540) 522-8823 cell


[log in to unmask]


www.gdit.com


<https://owandhm.gd-ns.com/exchweb/bin/redir.asp?URL=http://www.gdit.com


/>





________________________________





From: TechNet on behalf of Joel Alexander


Sent: Tue 5/29/2007 9:18 AM


To: [log in to unmask]


Subject: [TN] Fw: Status of IPC Solder Inspection Criteria











I apologize for the email chain but I wanted to get your opinions on


criteria for supported hole solder fill and pad wetting.  At the end of


the day I will provide the customer with what they want but I wanted to


get your opinions on the IPC-A-610 interpretations.

















---





Joe,





IPC do differentiate between wetting and solder fill.





   75% solder fill in the hole is acceptable


   180 degree top side wetting from lead to barrel is considered


   acceptable.


To clarify, the 75% fill is true as long as long you have wetting to the


top side lead to barrel transition and "0" wetting to the copper pad.














Eli,





For class 2 product, you need at least 180 degrees of circumferential wetting , observable in the hole, on the primary side. That solder, if properly wetted,  bonds the lead to the to the barrel in a supported hole confiquration. Note picture 7-115 on page 7-54 that shows 100% fill but a black ring around the lead. Just because you have solder present doesn't mean it is wetted or bonding the component to PTH barrel. That condition is a defect; because, it doesn't meet the 180 degrees wetting on lead or barrel.  The solder didn't bond to the finish on the lead (usually solderability, improper dwell, or thermal relief issues/heat sinking). Occasionally you will see that ring around the barrel...same defect...the solder didn't  bond/wet to barrel.





Since you only need 75% fill or the exception of 50% fill for thermal planes, no solder is required to be present on primary side pad.














Eli,





It  states lead to barrel not lead to land. If the fill requirement is


only


75%, then the land on the top side will not be wetted unless you have


100%


fill.








Joel Alexander


Quality Assurance Manager









































Joe,





What about section B














Lead to pad transition on the primary side.















































Eli,





I attached an extract from IPC-A-610 Rev D.  Wetting between the lead to


land is a Target condition and should not be cause for rejection.





Let me know if you want to discuss this further and Bill can set up a


conference call.
























































Elie, I forwarded your email to our Quality Manager.















































Bill,





There is  a misunderstanding of the way you interpret the acceptance


criteria of the lead-free solder connection vs. ours.  To my


knowledge, there should be  a wetting between the lead to pad transition


on


the component side of the board.  Your manufactured boards do not meet


this criteria.  Please let me know how we can resolve this issue?














ForwardSourceID:NT000B7562





---------------------------------------------------


Technet Mail List provided as a service by IPC using LISTSERV 15.0


To unsubscribe, send a message to [log in to unmask] with following text


in


the BODY (NOT the subject field): SIGNOFF Technet


To temporarily halt or (re-start) delivery of Technet send e-mail to


[log in to unmask]: SET Technet NOMAIL or (MAIL)


To receive ONE mailing per day of all the posts: send e-mail to


[log in to unmask]: SET Technet Digest


Search the archives of previous posts at:


http://listserv.ipc.org/archives


Please visit IPC web site


http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional


information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100


ext.2815


-----------------------------------------------------











---------------------------------------------------


Technet Mail List provided as a service by IPC using LISTSERV 15.0


To unsubscribe, send a message to [log in to unmask] with following text


in


the BODY (NOT the subject field): SIGNOFF Technet


To temporarily halt or (re-start) delivery of Technet send e-mail to


[log in to unmask]: SET Technet NOMAIL or (MAIL)


To receive ONE mailing per day of all the posts: send e-mail to


[log in to unmask]: SET Technet Digest


Search the archives of previous posts at:


http://listserv.ipc.org/archives


Please visit IPC web site


http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional


information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100


ext.2815


-----------------------------------------------------











---------------------------------------------------


Technet Mail List provided as a service by IPC using LISTSERV 15.0


To unsubscribe, send a message to [log in to unmask] with following text in


the BODY (NOT the subject field): SIGNOFF Technet


To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)


To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest


Search the archives of previous posts at: http://listserv.ipc.org/archives


Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815


-----------------------------------------------------











---------------------------------------------------


Technet Mail List provided as a service by IPC using LISTSERV 15.0


To unsubscribe, send a message to [log in to unmask] with following text in


the BODY (NOT the subject field): SIGNOFF Technet


To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)


To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest


Search the archives of previous posts at: http://listserv.ipc.org/archives


Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815


-----------------------------------------------------





Legal Disclaimer:

The information contained in this message may be privileged and confidential. It is intended to be read only by the individual or entity to whom it is addressed or by their designee. If the reader of this message is not the intended recipient, you are on notice that any distribution of this message, in any form, is strictly prohibited. If you have received this message in error, please immediately notify the sender and delete or destroy any copy of this message



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2