Michael,
QUESTION: at "normal" soldering iron temperatures, what happens when you
melt a eutectic solder preform (p/o clip lead) together with hi-temp, 90
to 94% Sn (bal=Pb) solder?
Will the two solders alloy, or just form a mixture? Please provide as
metallurgically correct an answer as possible.
Generally speaking, they will alloy. Issues that may impact the result
are things like:
melt (mixing) time
thermal (convection) gradients
flux activity
presence of oxides
presence of copper (intermetallics) from previous reflow cycles
Andy Magee
Flex Guru - Consulting
[log in to unmask]
(937) 435-3629
M.S.—Metallurgy—3.3 GPA—Univ. of Connecticut—1988
B.S.—Mechanical Engineering/Materials Engineering Dual Degree
Cum Laude—3.3 G.P.A—Univ. of Connecticut—1979
AESF, ASM, MRS, ASME
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|