Jiri,
We have our printers set to perform an automatic wiping operation after every 10th print. We tried 20, but cut our bridging by approximately 30% when we increased our frequency.
Leland Woodall
Quality Coordinator
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Ing.Jirí Janoch
Sent: Friday, August 26, 2005 7:52 AM
To: [log in to unmask]
Subject: [TN] Stencil cleaning in printers
Dear Techneters,
could you tell me, please, how often the stencil in a printer should be
cleaned automatically ?
I mean, how many PCBs could be paste-printed without stencil cleaning. Is it
a rule of thumb ?
Thanks for reply
J.Janoch
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|