TECHNET Archives

May 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Ofer Cohen <[log in to unmask]>
Date:
Thu, 12 May 2005 10:08:05 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joe Russeau <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Joe Russeau <[log in to unmask]>
Parts/Attachments:
text/plain (130 lines)
Hi Ofer,

I test PCB's all day long and I have found that powder-free vinyl gloves are
the ideal.  They are very clean and not likely to transfer harmful
contaminates.  As far as ESD is concerned, I have never personally had an
issue with using powder-free vinyl gloves on the ESD sensitive boards that I
have tested, but I also observe the appropriate grounding procedures before
handling such devices.  I am not aware of any specific glove that is
designed with ESD in mind, but that does not mean that one does not exist.
Personally, I am partial to the powder-free vinyl gloves for the work that I
do.  For those interested here is the part number of the gloves we use
PH2Y1952 and they come from VWR.  That part number is for a large glove ( I
need Large for my fat fingers), but they come in different sizes.

Best Regards,

Joe Russeau
Process Analyst

Precision Analytical Laboratory, Inc.
4106 Cartwright Dr. Ste. A
Kokomo, IN 46902

P: 765-455-1993
F: 765-455-1996
E: [log in to unmask]


----- Original Message -----
From: "Ofer Cohen" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, May 12, 2005 5:35 AM
Subject: Re: [TN] Gloves for handling Immersion Silver finished boards


> Most of the answers given are from PCB manufacturers, where ESD is not a
consideration. What gloves hould be used in the assembly house before and
after the reflow?
>
> Regards
>
> Ofer Cohen
> Seabridge
> A Siemens company
>
> > -----Original Message-----
> > From: TechNet [mailto:[log in to unmask]] On Behalf Of Kaye Clayo
> > Sent: Wednesday, May 11, 2005 19:53
> > To: [log in to unmask]
> > Subject: [TN] Gloves for handling Immersion Silver finished boards
> >
> > Hi Technet,
> >
> > Can anyone share what type of glove should be used when
> > handling immersion silver boards?
> >
> > If the immersion silver manufacturers say that rubber bands
> > are detrimental to the IAg finish, would latex gloves be bad also?
> > Are cotton gloves the answer?  Is there another type of glove
> > that is better?
> >
> > I have not been able to identify exactly what glove to use.
> > Or, maybe the type of glove is not even an issue?
> >
> > Thanks in advance,
> >
> > Kaye Clayo
> >
> > CONFIDENTIALITY NOTE: This message is intended only for the
> > use of the individual or entity to which it is addressed and
> > may contain information that is privileged, confidential, and
> > exempt from disclosure under applicable law. If the reader of
> > this notice is not the intended recipient, you are hereby
> > notified that any dissemination, distribution or copying of
> > this communication is strictly prohibited. If you have
> > received this communication in error, please notify the
> > sender immediately.
> >
> >
> >
> > ______________________________________________________________
> > _______________
> > Scanned by IBM Email Security Management Services powered by
> > MessageLabs. For more information please visit
> > http://www.ers.ibm.com
> > ______________________________________________________________
> > _______________
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a service by IPC using LISTSERV
> > 1.8e To unsubscribe, send a message to [log in to unmask] with
> > following text in the BODY (NOT the subject field): SIGNOFF
> > Technet To temporarily halt or (re-start) delivery of Technet
> > send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail
> > to [log in to unmask]: SET Technet Digest Search the archives
> > of previous posts at: http://listserv.ipc.org/archives Please
> > visit IPC web site
> > http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> > additional information, or contact Keach Sasamori at
> > [log in to unmask] or 847-615-7100 ext.2815
> > -----------------------------------------------------
> >
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
> -----------------------------------------------------
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2