The report claims that Tim Whiskers can be up to 9mm long and carry 10mA of
current...
That's quite a bit of amperage for a 1-2 micron whisker, I didn't know they
were that hearty.
Ken
Saturn PCB Design, Inc.
www.saturnpcb.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Buetow
Sent: Monday, May 23, 2011 2:14 PM
To: [log in to unmask]
Subject: [TN] New report finds tin whiskers to blame in Toyota UA
A new report is blasting the NASA and NHTSA reports on unintended
acceleration in Toyota vehicles, and specifically says tin whiskers is
among the culprits.
http://bit.ly/jDUofM
Best,
Mike
Mike Buetow
Circuits Assembly
w/m 617-327-4702
>>> The CIRCUITS ASSEMBLY EMS Directory -- over 2,100 listings, in Excel
www.circuitsassembly.com/dems <<<
Follow me on Twitter: twitter.com/mikebuetow
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|