TECHNET Archives

May 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 24 May 2005 08:28:06 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Wenger, George M." <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Wenger, George M." <[log in to unmask]>
Parts/Attachments:
text/plain (359 lines)
Kerry,

Is the BGA on the first side reflowed?  If so can it be tested without
doing the second side reflow?  This would help determine if the
intermittent is due to a "double reflow" type defect.

If your design engineers can determine the intermittent site or sites it
would be extremely helpful.  Intermittent interconnections are a real
problem to not only locate but to determine root cause.  It sounds like
you are going to have to do destructive cross sectioning to determine
the failure mode, which in turn will help in the root cause
determination.

Regards,
George
George M. Wenger, Andrew Corporation
Reliability / FMA Engineer
Base Station & Subsystems Group
40 Technology Drive, Warren, NJ 07059
(908) 546-4531 [log in to unmask]
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kerry McMullen
Sent: Tuesday, May 24, 2005 8:17 AM
To: [log in to unmask]
Subject: Re: [TN] BGA Intermittent

Hi Leo,
If pressure is applied to the part, the part functions (passes data).
When
the slight finger pressure is let off, the part fails (no data passes).






Leo Higgins <[log in to unmask]>
05/23/2005 05:31 PM

To
"'TechNet E-Mail Forum'" <[log in to unmask]>, "[log in to unmask]"
<[log in to unmask]>
cc

Subject
RE: [TN] BGA Intermittent






Can you define what you mean by "intermittent"?  Does this mean
measurements
on the same board show proper functionality but repeated measurements
show
that improper operation is sometimes noted?  How is this
measured....some
form of ICT?


Best regards,
Leo

Director of Applications Engineering
ASAT, Inc.
3755 Capital of Texas Highway, Suite 100
Austin, Texas     78704

ph     512-383-4593
fx      512-383-1590
[log in to unmask]
www.asat.com


The information contained in this electronic message is
CUSTOMER/SUPPLIER
PRIVILEGED AND CONFIDENTIAL INFORMATION intended only for the use of the
individual or entity named above. If the reader of this message is not
the
intended recipient, you are hereby notified that any dissemination,
distribution and copying of this communication is strictly prohibited.
If
you have received this communication in error, please immediately notify
the
sender by electronic mail. Thank you.



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Kerry McMullen
Sent: Monday, May 23, 2005 1:01 PM
To: [log in to unmask]
Subject: Re: [TN] BGA Intermittents


Hi Paul,
I am going to check now.  We have not had the problem before.

Kerry


Kerry McMullen
Principal New Product Mfg. Engineer
LTX Corporation
50 Rosemont Road
Westwood, MA 02090-2306
(T) 781-467-5468



Paul Edwards <[log in to unmask]>
05/23/2005 01:40 PM

To
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
cc

Subject
RE: [TN] BGA Intermittents






Kerry,

What size are the BGA pads and balls?

Paul Edwards
Process Engineering
[log in to unmask]
Tel: 408-433-4700
FAX: 408-433-9988
Surface Art Engineering
81Bonaventura Dr.
San Jose, CA 95134
DUNS: 944740570
CAGE/NCAGE: 1XZ48

-----Original Message-----
From: Kerry McMullen [mailto:[log in to unmask]]
Sent: Monday, May 23, 2005 10:31 AM
To: [log in to unmask]
Subject: Re: [TN] BGA Intermittents

Hi Technetters,
Typing too fast.
Balls are 63/37.  Ball temperature near the middle balls measured by
thermocouple is 206 Degrres C.  I do not want to go any higher as I
might
damage some of the other components on the board.  The board is 12" x
12"
double sided.    I'm not sure if the design engineers are creating a
fire
drill here, or not.   First they say its the middle.  Today it is the
corners.  The boards pass x-ray (non-oblique).    The boards have not
warped at all.  Very balanced board both in layer thickness and Cu
dispersion.    The only thing I have not found is the surface finish on
the BGA substrate.
I doubt it is the profile.....

Thanks in advance for your help.
Kerry





Bev Christian <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
05/23/2005 01:21 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Bev Christian <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] BGA Intermittents






Kerry,
Pure tin balls?!  I have not heard of that before.  Pure tin melts
considerably higher than SAC alloys.  Hmm, 206C you say, 14 layer board?
It is quite possible that your temperature/time is not enough to get a
significant amount of diffusional mixing of the solder paste and the
balls. But then you mention intermittents at the corners as well as the
center.

Two other possibilities are warping of the part (but would expect that
to
give you intermittents in one or the other area, not both) or there is a
severe problem with the construction of the component itself and there
is
internal damage to the component.

You don't say, but I presume the board itself solders well and there are
no other soldering problems on the board that would lead you to suspect
the solder paste?
Bev
RIM

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Kerry McMullen
Sent: May 23, 2005 1:10 PM
To: [log in to unmask]
Subject: [TN] BGA Intermittents


Hi Technetters,
I have a 1089 BGA with Sn balls.
Paste is 63/37 SnPb
Board is 14 layer,  .098 thick Immersion Ag.
Ran thermocouples.  Inner balls are seeing 206 degrees C.

What could be causing intermittents at the center and corners of the
BGA?

Thanks,

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
Kerry



---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public
information. Any use of this information by anyone other than the
intended
recipient is prohibited. If you have received this transmission in
error,
please immediately reply to the sender and delete this information from
your system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be
unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

------------------------------------------------------------------------------------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.  
If you have received it in error, please notify the sender
immediately and delete the original.  Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------------------------------
[mf2]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2