TECHNET Archives

January 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vqNdh-0000rrC; Fri, 31 Jan 97 12:24 CST
Content-Type:
text/plain; charset=US-ASCII
Old-Return-Path:
Date:
Fri, 31 Jan 1997 14:08:27 -0500
From [log in to unmask] Mon Feb 3 15:
22:42 1997
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
Content-Transfer-Encoding:
7bit
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/9834
TO:
Return-Path:
<TechNet-request>
X-Status:
Content-Description:
cc:Mail note part
Subject:
From:
X-Loop:
Mime-Version:
1.0
Resent-Message-ID:
<"3dde-.0.txM.eZZyo"@ipc>
Message-Id:
Parts/Attachments:
text/plain (53 lines)
     I use a CyberOptics Laser Section Microscope to measure solder paste 
     height on boards.  It can also be used to measure length and width and 
     hence be used to measure misregistration.  They can be reached at 
     (612) 542-5000.
     
     Linda Kenison
     Senior Process engineer
     Vicor
     (508)749-7570


______________________________ Reply Separator _________________________________
Subject: measuring paste height
Author:  [log in to unmask] at Internet
Date:    1/31/97 8:03 AM


     Can anyone reccommend a manufacturer of a device that measures
the height of solder paste after it is applied to the board.
                                                                                +



  Thanx Ahead
                                                                                +
  


     
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2