On December 9, John wrote:
>> Dan, you didn't mention if you bake before use. I suggest you have a
>> sample of each batch baked for at 2-4 hours at 220(F just before wave
>> solder and re-test. You may have a moisture problem.
John,
I was wondering though, if it were truly moisture related, wouldn't he be
seeing other stuff too after wave?...like some blowholes, voids, or junk
like that?
__\/__
. / ^ _ \ .
|\| (o)(o) |/|
#------.OOOo----oo----oOOO.-----#
# Steve Gregory #
# [log in to unmask] #
# #
#________________Oooo.__________#
.oooO ( )
( ) ) /
\ ( (_/
\_)
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|